Reflection Cracking at Joints

Description

Cracks in asphalt concrete overlay surfaces that occur over joints in concrete pavements.

Note: The slab dimensions beneath the AC surface must be known to identify reflection cracks at joints.

Severity Levels

Low
An unsealed crack with a mean width ≤ 6 mm; or a sealed crack with sealant material in good condition and with a width that cannot be determined.

Moderate
Any crack with a mean width > 6 mm and ≤ 19 mm; or any crack with a mean width ≤ 19 mm and adjacent low severity random cracking.

High
Any crack with a mean width > 19 mm; or any crack with a mean width ≤ 19 mm and adjacent moderate to high severity random cracking.

FIGURE 16 Distress Type ACP 5—Reflection
Cracking at Joints

How to Measure

Recorded as longitudinal cracking (ACP4) or transverse cracking (ACP6) on
LTPP surveys.

FIGURE 17 Distress Type ACP 5—High Severity Reflection Cracking at Joints